Rust on powder-coated steel parts: What can cause premature salt fog failures?

Q: I am looking at a report that a major company just sent in. The steel parts are showing signs...

Blisters and adhesion failure: Why is my powder coating failing salt spray and humidity tests?

Q: We are powder coating mild steel articles as follows: mild steel article + zinc plating (10 microns) + zinc...

Bubbling and chipping on dental equipment: Why is the epoxy/polyester powder coating bubbling and chipping off of my dental equipment?

Q: I am a dentist in Florida and am experiencing problems with the finish to my dental equipment. The equipment is...

Adhesion on automotive seat assembly brackets: Why is my powder coating chipping off my customer’s parts?

Q: I’m having a big problem with my powder coating chipping off my customer’s parts. These are automotive seat assembly...

Touching up wrinkle powder coating: Our touchup coat of wrinkle powder coating on HRPO steel is flaking off. What can we do?